Using photodiodes and supervised Machine Learning for automatic classification of weld defects in laser welding of thin foils copper-to-steel battery tabs

收藏
Zenodo2022-06-27 更新2026-05-25 收录
数据链接:
官方服务:

资源简介:

In this folder, excel files are stored with the results of signal processing that supported findings in the following paper: "Using photodiodes and supervised Machine Learning for automatic classification of weld defects in laser welding of thin foils copper-to-steell battery tabs". Matlab scripts and orginal signals will be uploaded soon with more detailed description.