Data supporting: 'Association between nanoscale strains and tissue level nanoindentation properties in age-related hip-fractures'

收藏
DataCite Commons2023-01-03 更新2025-04-09 收录
下载链接:
https://cord.cranfield.ac.uk/articles/dataset/Data_supporting_Association_between_nanoscale_strains_and_tissue_level_nanoindentation_properties_in_age-related_hip-fractures_/21806223/1
下载链接
链接失效反馈
官方服务:
资源简介:
Measurement of the properties of bone as a material can happen in various length scales in its hierarchical and composite structure. The aim of this study was to test the tissue level properties of clinically-relevant human bone samples which were collected from donors belonging to three groups: ageing donors who suffered no fractures (Control); untreated fracture patients (Fx-Untreated) and patient who experienced hip fracture despite being treated with bisphosphonates (Fx-BisTreated).