Research data supporting "Microstructural degradation of the AlMo0.5NbTa0.5TiZr refractory metal high entropy superalloy at elevated temperatures"

收藏
DataCite Commons2024-12-17 更新2024-08-25 收录
下载链接:
https://www.repository.cam.ac.uk/handle/1810/316457
下载链接
链接失效反馈
官方服务:
资源简介:
Data corresponding to the figures and tables in the associated paper. Data includes BSE SEM images, SEM EDX elemental distribution maps, SEM EDX quantitative measurements, and X-ray diffraction data.