Mechanical properties of single V2O5 nanocrystal - nanoindentation measurement in control of the max-depth
收藏Most Wiedzy Open Research Data Catalog2026-04-17 收录
下载链接:
https://mostwiedzy.pl/en/open-research-data/mechanical-properties-of-single-v2o5-nanocrystal-nanoindentation-measurement-in-control-of-the-max-depth,620025242642233-0
下载链接
链接失效反馈官方服务:
资源简介:
The DataSet contains the nanoindentation curves (indentation force Fn vs penetrationPd) for a single V2O5 nanocrystal supported on a substrate. The measurements were performed in control of the maximum depth of Berkovich indenter penetration: 60, 70, and 100 nm.
Nanoindentation curves were collected on a Nanoidenter TTX-NHT2 CSM. The details about measurements are included in each .text file.
提供机构:
Marta Prześniak-Welenc