five

Dataset for Machine learning assisted prediction of defects for laser powder bed fusion of nickel-based superalloy

收藏
NIAID Data Ecosystem2026-05-02 收录
下载链接:
https://data.mendeley.com/datasets/xr9tg6j7nx
下载链接
链接失效反馈
官方服务:
资源简介:
This document contains partial defect image processed by semantic segmentation model , deep learning code, binary model code, machine learning regression model code, and AM parameters with different defect datasets