Uniaxial creep test data for IN 939 material at 850 °C and a stress of 265 MPa

收藏
DataCite Commons2020-10-05 更新2025-04-16 收录
官方服务:

资源简介:

A collection of uniaxial creep data created at Henry Wiggin (now Special Metals Wiggin) in the context of a COST 50 Round I project to investigate the structural stability of nickel-base high temperature alloys.

创建时间:
2015-12-01