Pitting corrosion of AA1050 in ethanol-containing fuels: Classification dataset
收藏官方服务:
资源简介:
This dataset was used to predict the occurrence of ethanol-based pitting corrosion in AA1050 using binary classification. It consists of five system descriptors: Temperature (°C) Chloride content (ppm) Water content (ppm) Grit size of polishing paper Ethanol content (% by volume) of the fuel The target variable, named "corr," indicates corrosion occurrence, where 1 means corrosion occurred and 0 means no corrosion occurred. The dataset comprises 115 samples in total: 105 samples where corrosion occurred and 10 samples where no corrosion occurred.
提供机构:
Zenodo创建时间:
2024-08-08