Small punch creep test data for P92 material at 600 °C and a load of 475 N (specimen identifier BH-69)
收藏官方服务:
资源简介:
Content area for Swansea University data created in the scope of the small punch test standardization project.
创建时间:
2017-05-11

Content area for Swansea University data created in the scope of the small punch test standardization project.