Feasibility tests for DCT and PCT in Ni718 superalloy
收藏B2FIND2026-04-25 收录
下载链接:
https://b2find.eudat.eu/dataset/e1071fbc-46bd-51c2-9947-e3f2edb90e2e
下载链接
链接失效反馈官方服务:
资源简介:
A new batch of samples with different grain sizes (20 - 100 µm) and different precipitation states has been delivered for the upcoming InnovXN project. We will assess the...