Datasets (CSV files) from mechanical testing of fine-grained AZ31B magnesium alloy obtained by I-ECAP at 250 C and 200 C. Mechanical properties were investigated using an Instron 5969 testing machine with the maximum load capacity 50 kN. Tension and compression tests were carried out at room temperature with the initial strain rate equal to 1, 10-3 s-1. All specimens were cut out along ED. Flat tensile specimens, with thickness equal to 2 mm and dimensions of the gauge section 2.5 mm, 14 mm, were machined using wire electrical discharge machining (EDM).Height and diameter of the compression specimens were 8 mm and 7 mm, respectively. This dataset relates to the EPSRC funded SAMULET Project 4 Task 4.3.1 and Task 4.3.2 (EP/G03477X/1).
提供机构:
University of Strathclyde
创建时间:
2015-03-19
5,000+
优质数据集
54 个
任务类型
进入经典数据集
二维码
社区交流群

面向社区/商业的数据集话题

二维码
科研交流群

面向高校/科研机构的开源数据集话题

数据驱动未来

携手共赢发展

商业合作