Uniaxial creep test data for P91 nt material at 600 °C and a stress of 180 MPa (specimen identifier G91-5)
收藏官方服务:
资源简介:
The present test data sets have been generated by KAERI in the scope of the MATTER project.
创建时间:
2015-06-12

The present test data sets have been generated by KAERI in the scope of the MATTER project.