Experimental dataset for CoNi-based superalloys high-temperature creep behavior study
收藏NIAID Data Ecosystem2026-05-10 收录
官方服务:
资源简介:
This dataset contains raw and processed data supporting the findings of this study, including microstructure images SEM and TEM data.
创建时间:
2026-03-27