遇见数据集

Nanoindentation study on the phase transformation of single crystal silicon of different crystallographic orientations using a spherical indenter probe

收藏
data.gov2025-12-20 收录
官方服务:

资源简介:

The effect of the crystallographic orientation on the primary and secondary phase transformations of single-crystal silicon (Si) during indentation was investigated...