Uniaxial creep test data for ER 316L sa wm material at 550 °C and a stress of 402 MPa (specimen identifier 36319)
收藏官方服务:
资源简介:
Data created by ENEA, Italy during the Horizon 2020 GEMMA project on GenIV materials maturity, including test results from an SSRT round-robin on EUROTRANS/DEMETRA T91 in Pb at 400°C. This project has received funding from the Euratom research and training programme 2014-2018 under Grant Agreement No. 755269.
创建时间:
2022-06-08