资源简介:

Design of a novel Ni-based superalloy for additive repair application using neural network optimisation. This data set includes the raw files for the test methods used for this manuscript. The test methods include: XRD, TGA and DSC. These data are included as text files and can be read into any appropriate software.

创建时间:
2022-08-09