IV sweeps raw data for POM film humidity and CO2 testing
收藏DataCite Commons2023-11-21 更新2024-07-13 收录
下载链接:
https://data.ncl.ac.uk/articles/dataset/IV_sweeps_raw_data_for_POM_film_humidity_and_CO2_testing/24449584
下载链接
链接失效反馈官方服务:
资源简介:
IV measurements were performed between -2 V and 2 V with a step size of 0.1 V. Measurements were taken in the forward and reverse direction. The resistance of the device was calculated through the inverse slope of the resultant linear line from which the conductivity was calculated using equation 4.1. The length and width of the channel were measured with an optical microscope.R=V/I=ρ(L/A) σ=1/ρWhere σ: conductivity, ρ: resistivity, R: resistance in ohms, L: length in metres, A: the area in m<sup>2</sup>, V: voltage, and I: current.Samples were measured in a humidity-controlled environment with a purpose-built holder and printed circuit board (PCB), and a water bubbler to control humidity coupled with a QTenki humidity sensor and temperature probe (Dracal Technologies). Four repeat measurements were taken for each POM electrode.
提供机构:
Newcastle University
创建时间:
2023-11-21