Nanoindentation data set: Calibration and data analysis routines for nanoindentation with spherical tips
收藏NIAID Data Ecosystem2026-03-14 收录
下载链接:
https://zenodo.org/record/7607546
下载链接
链接失效反馈官方服务:
资源简介:
These data comprise of nanoindentation experiements, which are described and analysed in the manuscript: Calibration and data analysis routines for nanoidentation with spherical tips.
创建时间:
2023-02-06