Intergranular strain formation in Nickel based superalloys close to the yield...
收藏B2FIND2026-04-25 收录
下载链接:
https://b2find.eudat.eu/dataset/3af7e2c7-e11f-559a-ab47-72cb0e91471b
下载链接
链接失效反馈官方服务:
资源简介:
Nickel based superalloys retain high strength up to high temperatures and are therefore often used in gas turbines. Here, hardening mechanisms and their respective supersessions...