Data supporting this article includes electrochemical tests, X-ray diffraction, and SEM images. This project was studying the effects of different cycling procedures on the lifetime of Li-O2 batteries. In particular, the differences between purely constant current cycling and constant current discharge followed by constant current + potential hold (until current drops to 10% of original current) was investigated. The Li-O2 cells studied were all cycled 10 times with a capacity limitation of 1 mAh/cm2. They had 1 M LiTFSI in DME electrolyte. The cycling conditions were: - Constant current discharge and charge, upper cutoff voltage (UCV) 3.5 V, 3.8 V and 4 V - Constant current discharge and constant current + potential hold charge, UCV 3.5 V, 3.8 V and 4 V - Constant current discharge and constant current + potential hold charge, LiI redox mediator in electrolyte (5 mM), UCV 3.4 V, 3.5 V, 3.8 V Electrochemical data are .xlsx files generated by Arbin cycler, XRD data with Cu source of air electrodes from cells mentioned above SEM images of the air electrodes mentioned above
提供机构:
Apollo - University of Cambridge Repository
创建时间:
2025-01-09
5,000+
优质数据集
54 个
任务类型
进入经典数据集
二维码
社区交流群

面向社区/商业的数据集话题

二维码
科研交流群

面向高校/科研机构的开源数据集话题

数据驱动未来

携手共赢发展

商业合作