遇见数据集

Research data supporting "Exploration of potential-limited protocols to prevent inefficiencies in Li–O2 batteries during charge"

收藏
DataCite Commons2025-05-08 更新2025-05-10 收录
官方服务:

资源简介:

Data supporting this article includes electrochemical tests, X-ray diffraction, and SEM images. This project was studying the effects of different cycling procedures on the lifetime of Li-O2 batteries. In particular, the differences between purely constant current cycling and constant current discharge followed by constant current + potential hold (until current drops to 10% of original current) was investigated. The Li-O2 cells studied were all cycled 10 times with a capacity limitation of 1 mAh/cm2. They had 1 M LiTFSI in DME electrolyte. The cycling conditions were: - Constant current discharge and charge, upper cutoff voltage (UCV) 3.5 V, 3.8 V and 4 V - Constant current discharge and constant current + potential hold charge, UCV 3.5 V, 3.8 V and 4 V - Constant current discharge and constant current + potential hold charge, LiI redox mediator in electrolyte (5 mM), UCV 3.4 V, 3.5 V, 3.8 V Electrochemical data are .xlsx files generated by Arbin cycler, XRD data with Cu source of air electrodes from cells mentioned above SEM images of the air electrodes mentioned above

创建时间:
2025-01-09
二维码
社区交流群
二维码
科研交流群
商业服务