Enhanced strength-ductility and stress-rupture properties of a Ni-based superalloy via nanotwins and stable γ’ particles
收藏Figshare2025-12-08 更新2026-04-28 收录
下载链接:
https://figshare.com/articles/dataset/Enhanced_strength-ductility_and_stress-rupture_properties_of_a_Ni-based_superalloy_via_nanotwins_and_stable_particles/30824076
下载链接
链接失效反馈官方服务:
资源简介:
Here, we alter the alloying elements of GH4742 superalloy by means of domain-knowledge informed thermodynamic calculation to reduce the stacking fault energy of the γ matrix and enhance the stability of γ’ particles. Increasing Co and Cr concentrations with Mo substitution by W induces the formation of high-density stacking faults and nanotwins, while reducing the coarsening rate of γ’ particles during tensile testing at 760°C and stress-rupture loading at 760°C/480 MPa. Thus, the yield strength, working-hardening capacity, and stress-rupture life are simultaneously improved, achieving the synergic enhancements in strengths-ductility and stress-rupture properties at elevated temperature.
创建时间:
2025-12-08