Dataset of comprehensive Full-notch creep tests (FNCT) of selected high-density polyethylene (PE-HD) materials

收藏
Zenodo2023-11-16 更新2026-04-07 收录
官方服务:

资源简介:

The dataset provided in this repository comprises data obtained from a series of full-notch creep tests (FNCT) performed on selected high-density polyethylene (PE-HD) materials (for further details, see section 1 Materials in this document) in accordance with the corresponding standard ISO 16770 [1]. The FNCT is one of the mechanical testing procedures used to characterize polymer materials with respect to their environmental stress cracking (ESC) behavior. It is widely applied for PE-HD materials, that are predominantly used for pipe and container applications. It is based on the determination of the time to failure for a test specimen under constant mechanical load in a well-defined and temperature controlled liquid environment. The test device used here also allows for continuous monitoring of applied force, specimen elongation and temperature.

创建时间:
2023-11-16
二维码
社区交流群
二维码
科研交流群
商业服务