In situ Investigation of structural degradation of LiCo0.15Ni0.85O2 and LiFePO4 cathode materials

收藏
Research Data Australia2024-12-14 收录
下载链接:
https://researchdata.edu.au/in-situ-investigation-cathode-materials/341458
下载链接
链接失效反馈
官方服务:
资源简介:
Samples: lithium iron phosphate (LiFePO4) lithium cobalt oxide (LiCoO2) graphite (C) ethylene carbonate Lithium nickel oxide (LiNiO2) copper (Cu) aluminum (Al) lithium hexafluorophosphate (LiPF6) polyethylene dimethyl carbonate D6 Analysis of the sample(s) listed above by the instruments at the Australian Nuclear Science and Technology Organisation. Investigators: * Professor Zhaoxiang Wang (zxwang@aphy.iphy.ac.cn) * Dr Zaiping Guo (zaiping_guo@uow.edu.au) * Dr Shulei Chou (sc478@uow.edu.au) * Dr Jiazhao Wang (jiazhao@uow.edu.au) * Lanyao Shen (shenlanyao@163.com) * Mr Neeraj Sharma (njs@ansto.gov.au)
提供机构:
Australian Nuclear Science and Technology Organisation
5,000+
优质数据集
54 个
任务类型
进入经典数据集
二维码
社区交流群

面向社区/商业的数据集话题

二维码
科研交流群

面向高校/科研机构的开源数据集话题

数据驱动未来

携手共赢发展

商业合作