Small punch creep test data for 14 Cr 1 W ods material at 650 °C and a load of 130 N (specimen identifier D2-3)

收藏
DataCite Commons2024-10-15 更新2025-04-16 收录
官方服务:

资源简介:

After analysing the running projects on different innovative reactor and transmutation systems and their related needs in terms of structural materials assessment, the focus of GETMAT has been put on F/M and ODS steels, as cross-cutting structural material choice for core and primary components. Moreover, the GETMAT project aims as well to streamline and integrate, in a comprehensive way, the R&D effort of the European materials laboratories for a wide-range study of the performance of the two classes of alloys, in terms of (i) availability, fabricability and fundamental properties, (ii) compatibility with coolants and (iii) response to irradiation, including (iv) an effort to understand the physical reasons for their behaviour under these conditions. In detail, the priorities and objectives GETMAT are: - Improvement and extension of 9-12 Cr F/M steels qualification - ODS alloys development and characterisation - Joining and welding procedures qualification (relevant for both ODS and F/M steels) - Development and definition of corrosion protection barriers - Improved modelling and experimental validation. Our contribution to the project was the mechanical characterisation of a 14 Cr ODS steel and a 9 Cr ODS steel by means of small punch and uniaxial creep as well as low cycle fatigue tests at elevated temperature.

创建时间:
2013-05-31
二维码
社区交流群
二维码
科研交流群
商业服务