Supplementary nanoindentation data on PVD sputter-deposited MoS2 coatings

收藏
Zenodo2021-06-11 更新2026-05-25 收录
数据链接:
官方服务:

资源简介:

This data publication contains the results of nanoindentation tests on magnetron-sputtered MoS<sub>2</sub> coatings and supplements the publication “Microstructure, mechanical properties and tribological behavior of magnetron-sputtered MoS<sub>2</sub> solid lubricant coatings deposited under industrial conditions” doi: 10.3390/coatings10080755. The coatings are described in the zenodo publication “Tribological investigations of PVD-MoS<sub>2</sub> coatings on a ball-on-disk tribometer under vacuum conditions” doi: 10.5281/zenodo.4903434. Please refer to their file "All_samples.csv" for the deposition parameters of the different samples. The current publication takes over the sample naming convention. Nanoindentations were performed by S.Krauß under the supervision of B.Merle at the Institute I of the Materials Science and Engineering Department of the Friedrich-Alexander University Erlangen-Nürnberg (Martensstr.5, 91058 Erlangen, Germany) using a G200 nanoindenter (KLA, Milpitas, CA, USA), equipped with a Berkovich diamond indenter tip. 25 nanoindentations were performed on each coating in Continuous Stiffness Measurement mode. The maximum indentation depth was 500 nm . Because of the strongly different coating thicknesses, the indentation hardness and indentation modulus were evaluated in the range 4 - 6 % of the individual coating thickness. The data are provided in 43 .csv files, each corresponding to a single coating. The data in each .csv file are organized as follows: There are 27 rows in each file. Each row contains seven comma separated characters, forming seven columns. The data description is given in row 1, e.g., “Hardness”. The physical unit is given in row 2, e.g., “GPa”. From row 3 to row 27, the individual measurement values are provided for the respective indents. The following information can be found in the respective columns: 1: Test number. 2: Indentation modulus in GPa. 3: Indentation hardness in GPa. 4:Drift correction during experiment in nm/s. 5: Time of the measurement. 6: Tip-calibration-function used for evaluation. 7: Temperature during the measurement in °C.

提供机构:
Zenodo
创建时间:
2021-06-11
二维码
社区交流群
二维码
科研交流群
商业服务