Analyses of deuterium retention in tungsten and graphite first wall materials by laser-induced ablation spectroscopy on EAST
收藏科学数据银行2022-11-24 更新2026-04-23 收录
下载链接:
https://www.scidb.cn/detail?dataSetId=5661b872e914477ab81918c16b9793f1
下载链接
链接失效反馈官方服务:
资源简介:
Plasma-wall interactions at the first wall in fusion experimental devices are critical for the life time of plasmafacing components and tokamak operation. In-situ measurements of these plasma-wall interaction processes are required in long pulse devices in order to understand better the underlying mechanisms as well as monitoring of the tritium content of the first wall as an immediate safety application. In this work we present measurements of the deuterium retention in the first wall of EAST using laser-induced ablation spectroscopy. The diagnostic is applied during plasma operation and the dynamic retention for graphite and tungsten as plasma-facing materials are compared, showing more than three times higher short-term retention in graphite than in tungsten. Laserbased analysis is applied during a shift of the vertical positions of the plasma column in limited as well as in the start-up phase of discharges in diverted magnetic configuration. Plasma core densities of n e = (1.5–3.2) × 10 19 /m3 are chosen to vary the ion flux to the first wall and study saturation effects of deuterium on the surface first wall materials during tokamak plasma operation. A linear dependence of the retention from ion fluence is observed for graphite as PFC up to 3 × 10 18 D+ /cm2 , followed by a constant retention up to fluences of 3.5 × 1019 D+ /cm2 for nearby first wall temperatures of T PFC ≈ 350 K.
提供机构:
Guangnan Luo; Hefei Institutes of Physical Science; Jiamin Liu; Institute of Plasma Physics; Hongbin Ding; Forschungszentrum Julich GmbH; Junlin Chen; Dalian University of Technology; Liying Sun
创建时间:
2022-10-14