XRD, particle sizing, electrochemistry, nanoindentation and impedance datasets for research paper
收藏官方服务:
资源简介:
CRB12 = NMC811-radial CRB17 = NMC811-random Some XRD-CT and XRF-CT publicly available at https://doi.esrf.fr/10.15151/ESRF-ES-502906467. Full data available via request to authors.
提供机构:
Zenodo创建时间:
2025-02-25