Research data for the research titled, "Hand-Held Laser Welding of Grade-2 Titanium: Effects of Enhanced Shielding on Fractography, Microstructure, and Mechanical Properties"
收藏Mendeley Data2026-04-09 收录
官方服务:
资源简介:
This is research data for the research titled, "Hand-Held Laser Welding of Grade-2 Titanium: Effects of Enhanced Shielding on Fractography, Microstructure, and Mechanical Properties".