Data for: Establishment of damage statistical constitutive model of loaded rock and method for determining its parameters under freeze-thaw condition
收藏NIAID Data Ecosystem2026-03-10 收录
下载链接:
https://data.mendeley.com/datasets/jcz6wdfjxh
下载链接
链接失效反馈官方服务:
资源简介:
No. 3-3 refers to the sample after 0 cycles of freeze-thaw, No. 3-5 refers to the sample after 10 cycles of freeze-thaw, No. 3-9 refers to the sample after 15 cycles of freeze-thaw, No. 3-11 refers to the sample after 20 cycles of freeze-thaw, No. 3-15 refers to the sample after 25 cycles of freeze-thaw, No. 3-18 refers to the sample after 30 cycles of freeze-thaw.
创建时间:
2019-01-22