资源简介:

TC4 specimen thickness δ= 7 mm, with an error of ± 0.1mm. Test the non LSP specimens and the LSP8, LSP10, and LSP12 specimens subjected to impact strengthening at laser power densities of 8 GW/cm2, 10 GW/cm2, and 12 GW/cm2, respectively. Residual stress test results