The XRD diffraction patterns of La0.3Sr0.6Ce0.1Ni0.1Mo0.9O3-s powder calcined at 800oC in H2
收藏Most Wiedzy Open Research Data Catalog2026-04-17 收录
下载链接:
https://mostwiedzy.pl/en/open-research-data/the-xrd-diffraction-patterns-of-la0-3sr0-6ce0-1ni0-1mo0-9o3-s-powder-calcined-at-800oc-in-h2,616041253653222-0
下载链接
链接失效反馈官方服务:
资源简介:
The dataset includes XRD patterns of La0.3Sr0.6Ce0.1Ni0.1Mo0.9O3-s powder prepared using wet chemistry methods, namely modified Pechini route. The powders were sintered at 800oC for 12 h in H2. Pure perovskite phase was formed
提供机构:
Patryk Błaszczak