Uniaxial creep test data for Model Alloy (Fe-9Cr) ar material at 590 °C and a stress of 178 MPa (specimen identifier FO-08)

收藏
DataCite Commons2024-07-17 更新2025-04-16 收录
官方服务:

资源简介:

Data from the Open Access to JRC Research Infrastructures SCS project between SCK CEN and European Commission JRC, whereby SCK CEN made use of JRC Petten facilities to perform screening creep tests for the recently developed advanced grades of EUROFER97 steel, which is a task that lies within a global objective to develop the reduced activation ferritic/martensitic steel for high temperature applications with enhanced creep strength and irradiation resistance, which is pursued under EU-scale research in Fusion and Fission domains.