Nanoindentation data/code for anodic coating on additively manufactured Al10SiMg alloy

收藏
NIAID Data Ecosystem2026-05-01 收录
官方服务:

资源简介:

Experimental nanoindentation data for anodic coating on additively manufactured Al10SiMg. Data from nanoindentation experiments conducted on plan- and cross-sections of additively manufactured (AM) Al-10Si-Mg alloy was considered for modelling. Apart from nanomechanical properties, load and displacement curves were predicted using Python software from ANN and the power law models. The ANN and power law models can predict elastic modulus and hardness at different loads by conducting the minimum number of experiments.

创建时间:
2024-04-03