Nanoindentation (single cycle) test data for Fused silica ar material at 23 °C and maximum indenter force of 10.031 mN (first nominally repeat test)
收藏官方服务:
资源简介:
Data created at the European Commission JRC during the CEN Workshop NATEDA on nanoindentation test data, itself a component of the H2020 M4F project funded from the Euratom research and training programme 2014-2018 under grant agreement No. 755039.