The dataset includes the TPR reduction profiles of Ce0.9M0.1O2 (where M=Mn, Fe, Co, Ni, Cu) nanopowders prepared by the reverse microemulsion method. After the synthesis powders were dried, then calcined at 500 degrees for 2 h. The measurements were carried out in H2/Ar mixture from 100C to 900C. Gas flow:40ml/min and temperature ramp: 10deg/min.