Mechanism of Ca2+, Mg2+ and Fe3+ in fine cassiterite flotation using octanohydroxamic acid
收藏资源简介:
The existence of metal ion should not be ignored in both hydrometallurgy and flotation. In this study, the effects of Ca2+, Mg2+ and Fe3+ on the flotation performance of cassiterite using octanohydroxamic acid (OHA) as the collector were investigated by the micro-flotation tests, X-ray photoelectron spectroscopy (XPS), fourier transform infrared spectroscopy (FTIR), contact angle, zeta (ζ) potential measurements and atomic force microscopy (AFM) imaging. The results of the flotation and contact angle experiments showed that the addition of Ca2+, Mg2+ and Fe3+ significantly decreased both the recovery and contact angle of cassiterite within pH ranged from 6.0 to 12.0 in the presence of OHA collector. ζâpotential measurements, solution chemistry analysis and FTIR measurements indicated that the flotation recovery of the cassiterite declined due to the CaOH+, MgOH+ and Fe(OH)3 sites on the cassiterite surface. XPS results indicated that the chemisorption of OHA on cassiterite surface and i...