In this folder, excel files are stored with the results of signal processing that supported findings in the following paper: "Using photodiodes and supervised Machine Learning for automatic classification of weld defects in laser welding of thin foils copper-to-steell battery tabs". Matlab scripts and orginal signals will be uploaded soon with more detailed description.