遇见数据集

Research data supporting "An investigation of the miscibility gap controlling phase formation in refractory metal high entropy superalloys via the Ti-Nb-Zr constituent system"

收藏
DataCite Commons2024-12-17 更新2024-08-25 收录
官方服务:

资源简介:

Data corresponding to the figures and tables in the associated paper. Data includes BSE SEM images, SEM EDX elemental distribution maps, TEM HAADF images, TEM diffraction patterns, STEM EDX elemental distribution maps and x-ray diffraction data.

创建时间:
2021-07-19
二维码
社区交流群
二维码
科研交流群