five

Electrodeposition of Composite Coatings of Cu/AlO(OH) Using Allyl Alcohol as an Additive

收藏
DataCite Commons2020-08-29 更新2024-07-27 收录
下载链接:
https://scielo.figshare.com/articles/Electrodeposition_of_Composite_Coatings_of_Cu_AlO_OH_Using_Allyl_Alcohol_as_an_Additive/6151799
下载链接
链接失效反馈
官方服务:
资源简介:
In this work, composite coatings of Cu/AlO(OH) were produced by electrodeposition on steel substrates using a pyrophosphate-based bath containing allyl alcohol as an additive. The electrodeposition of the composite coatings was carried out using a 23 central composite design (CCD), aiming to verify the effects of the deposition parameters (previous stirring time (t), the stirring speed (S) and the current density (j)), considered the entry variables, on the electrochemical behavior of Cu/AlO(OH) coating, the response variables of the CCD. The results indicated that a decrease of the parameters j and S directly influenced the values of Rp and Rct, leading to the production of protective coatings. The best result (Rp = 211 Ω and Rct = 221 Ω) was obtained under conditions where t = 120 min, S = 1300 rpm and j = 7 A m-2. Dispersed bohemite particles could be noted on the surface of the composite coating.
提供机构:
SciELO journals
创建时间:
2018-04-18
5,000+
优质数据集
54 个
任务类型
进入经典数据集
二维码
社区交流群

面向社区/商业的数据集话题

二维码
科研交流群

面向高校/科研机构的开源数据集话题

数据驱动未来

携手共赢发展

商业合作