Raw data of the creep tests on cylindrical specimens
收藏资源简介:
This dataset contains the raw data of the creep tests on the concrete cylinder specimens. Four batches (batch 1 and 2 of concrete C80 and batch 3 and 4 on concrete C30) were tested. Three specimens were placed on top of each other in each test and loaded with the same load. The specimens are referenced with letters O (top), M (middle) and U (bottom). Following measuring channels are used in each file: - Zeit (time) in s - Umgebungstemperatur (ambient temperature) in °C - Luftfeuchtigkeit (relative humidity) in % - Kraft (force) in kN - Verformung bei Umfang (displacement at circumference) 0° in mm - Verformung bei Umfang (displacement at circumference) 120° in mm - Verformung bei Umfang (displacement at circumference) 240° in mm - Mittelweg der drei Verformungen (average value of the three displacements) in mm