High resolution deformation data from the surface of a Nickel-based superalloy: Fine precipitates

收藏
Zenodo2022-10-24 更新2026-05-25 收录
数据链接:
官方服务:

资源简介:

High resolution digital image correlation (HRDIC) and electron backscattered diffraction (EBSD) data provided that quantifies the deformation on the surface of Nickel-based superalloy with fine gamma prime precipitates (70 nm diameter) after 2% strain in tension.