five

Corrosivity Caused by Salt Solutions Employed in the Wood Dimensional Stability

收藏
Figshare2017-03-01 更新2026-04-29 收录
下载链接:
https://figshare.com/articles/dataset/Corrosivity_Caused_by_Salt_Solutions_Employed_in_the_Wood_Dimensional_Stability/5670337
下载链接
链接失效反馈
官方服务:
资源简介:
ABSTRACT The study aimed to evaluate the corrosivity of salt solutions after and before the impregnation in the wood. Solutions with concentration of 5% of chloride of lithium, sodium carbonate, magnesium sulphate, zinc sulphate and copper sulphate II had been kept during 6 hours, at 25; 45 and 100 °C, in contact with steel plates carbon samples of 1.25 × 0.1 × 7.5 cm (width × thickness × length), before and after its contact with wood samples of Corymbia torelliana and Eucalyptus cloeziana. There was no effect of the temperature in the corrosion of the pure solutions. After the contact with woods, corrosivity was incremented with copper II and zinc sulphate solutions. Copper II sulphate caused the biggest loss of mass in plates, and its contact with metallic surfaces is not recommended as wood treatment and drying chambers.
创建时间:
2017-03-01
5,000+
优质数据集
54 个
任务类型
进入经典数据集
二维码
社区交流群

面向社区/商业的数据集话题

二维码
科研交流群

面向高校/科研机构的开源数据集话题

数据驱动未来

携手共赢发展

商业合作