High resolution deformation data from the surface of a Nickel-based superalloy: Fine precipitates
收藏数据链接:
官方服务:
资源简介:
High resolution digital image correlation (HRDIC) and electron backscattered diffraction (EBSD) data provided that quantifies the deformation on the surface of Nickel-based superalloy with fine gamma prime precipitates (70 nm diameter) after 2% strain in tension.
创建时间:
2020-02-28