BAM reference data: results of ASTM E139 -11 creep tests on a reference material of Nimonic 75 nickel-base alloy
收藏数据链接:
官方服务:
资源简介:
Results of creep tests on a certified reference material at T = 600°C and a tensile creep load of 160 MPa are provided. The raw data are available in ASCII format (*.lis files). <br> The file "Inhalt_Content_V1.1.pdf" contains further information about the files provided.<br> The evaluated results include the times to reach 2% and 4% creep strain, respectively, and the creep rate after 400 h. The tests were carried out in an accredited test laboratory. The calibrations of all measurands and test and measuring equipment are documented. The calibrations meet the requirements of the test procedure and are metrologically traceable.