遇见数据集

Binary III-V Semiconductor Plasma Etch Rates

收藏
NIAID Data Ecosystem2026-05-02 收录
官方服务:

资源简介:

Etch rate data gathered from plasma etching results reported in the literature for the main binary III-Vs. This dataset provides detailed information on the plasma etching of binary III-V semiconductors reported in the literautre. Each entry is identified by the last name of the first author and publication date and includes a link to the source or publication, the III-V material that was etched, the technique used for etching, the main chemical etchant(s) used, and the associated etch rate or range of etch rates. Etch rates were either extracted directly from the text or obtained by digitizing figures.

创建时间:
2025-05-14
二维码
社区交流群
二维码
科研交流群
商业服务