Casting voids in nickel superalloy and the mechanical behaviour under room temperature tensile deformation
收藏Mendeley Data2024-03-27 更新2024-06-28 收录
下载链接:
https://zenodo.org/record/4432446
下载链接
链接失效反馈官方服务:
资源简介:
This repository contains the original X-ray tomography data presented in the publication 'Casting voids in nickel superalloy and the mechanical behaviour under room temperature tensile deformation'. The XCT data were collected using Zeiss Xradia Versa 520 instrument from Henry Moseley X-ray Imaging facility at the University of Manchester. Access to the instrument was granted by Henry Royce Institute through PhD access funding scheme for Zhuocheng Xu. Data to produce Figure8 and Figure9 are also uploaded.
创建时间:
2023-06-28