遇见数据集

Uniaxial creep test data for P91 ar material at 375 °C and a stress of 415 MPa (specimen identifier MC-07)

收藏
DataCite Commons2023-10-20 更新2025-04-16 收录
官方服务:

资源简介:

The 2010-2012 implementation plan of the European Sustainable Nuclear Industrial Initiative (ESNII), in the frame of the Sustainable Nuclear Energy Technology Platform (SNE TP), establishes a very tight time schedule for the start of construction of the European Gen IV prototypes; namely the construction of the LFR ETPP (European Technology Pilot Plant) Myrrha will start in 2014 and that of the SFR Prototype ASTRID will start in 2017. The GEN IV reactors pose new challenges to the designers and scientists in terms of higher operating temperature and higher irradiation damage of materials with respect to the present technologies. In this frame, the MATTER (MATerials TEsting and Rules) Project intends to start well targeted researches to perform careful studies of materials behaviors in GEN IV operational conditions and to find out criteria for the correct use of these materials in relevant reactor applications. In that context, the JRC has carried out different tests (LCF, Creep, Small Punch Creep, Small Punch Tensile/Fracture) tests on P91 and 316. The activities were carried out in the frame of the MATTER project (Grant agreement no: 269706).

创建时间:
2014-11-21
二维码
社区交流群
二维码
科研交流群
商业服务