Light intensity in reflection mode of PAAO (1st sample 1st anodization)
收藏NIAID Data Ecosystem2026-05-01 收录
数据链接:
官方服务:
资源简介:
Light intensity data recorded during the anodization of aluminum polycrystal. Light source: SLS201L/M (ThorLabs). Spectrometer: USB4000 (OceanOptics). Spectra acquisition software: SpectraSuite (OceanOptics). Integration time: 340 us. Scans to average: 5. Spectrum is recorded every 1 s during anodization. ref.txt includes reference spectra before the start of anodization process. Anodization was performed in 0.3 mol/L oxalic acid at 40 V for 1 hour.
创建时间:
2023-06-30