Computational Data - Role of Molecular Orientation: Comparison of Nitrogenous Aromatic Small Molecule Inhibitors for Area-Selective Atomic Layer Deposition

收藏
NIAID Data Ecosystem2026-05-02 收录
数据链接:
官方服务:

资源简介:

Area-selective atomic layer deposition (AS-ALD) shows great potential for meeting the stringent demands of the semiconductor industry for precision nanopatterning. Small molecule inhibitors (SMIs) have recently proven to be a promising, industry-compatible means of achieving AS-ALD. In this work, we compare three nitrogenous aromatic SMIs – aniline, pyrrole, and pyridine – for their ability to block Al2O3 ALD on copper with (CuOx) and without (Cu) a native oxide. We find that pyrrole and aniline perform much better as inhibitors than does pyridine. Furthermore, when redosed on copper before every ALD cycle in an ABC scheme, pyrrole and aniline provide outstanding inhibition, facilitating the selective deposition of over 11 nm of Al2O3 on an SiO2 growth surface in the presence of Cu with 99.9% selectivity. By combining both theory and experiment, we provide new understanding of the mechanisms by which selectivity is prolonged and lost. First, we show that the CuOx surface is inherently more reactive than the Cu surface, leading to an eventual loss of selectivity, even when the inhibitor is redosed. Second, we find that whereas pyrrole and aniline adsorb in a planar bonding orientation, pyridine binds upright at the copper surface and we propose that the upright orientation is the origin of the ineffective inhibition of pyridine. Finally, we observe that redosing of aniline protects the copper surface from undesired oxidation, whereas the redosing of pyridine does not. As such, we posit that a likely benefit of redosing is preventing oxidation and thus reducing reactive site formation during ALD. Through this work, we demonstrate the capability of nitrogenous aromatics to serve as SMIs for AS-ALD, and we contribute valuable insights regarding the impact of ALD process parameters on selectivity.

创建时间:
2024-10-01
二维码
社区交流群
二维码
科研交流群
商业服务