XRD, particle sizing, electrochemistry, nanoindentation and impedance datasets for research paper
收藏NIAID Data Ecosystem2026-05-02 收录
下载链接:
https://zenodo.org/record/14925159
下载链接
链接失效反馈官方服务:
资源简介:
CRB12 = NMC811-radial
CRB17 = NMC811-random
Some XRD-CT and XRF-CT publicly available at https://doi.esrf.fr/10.15151/ESRF-ES-502906467. Full data available via request to authors.